Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 2160 cP

@Temperature 40.0 °C
2160 cP

@Temperature 104 °F
BASF Pluracol® 4600 Graft Slabstock Foam Polyol
Description: Pluracol® 4600 polyol is a secondary hydroxyl-terminated graft polyether triol containing approximately 44% solids of copolymerized styrene and acrylonitrile. This polyol has been form..
Viscosity 2160 cP

@Temperature 40.0 °C
2160 cP

@Temperature 104 °F
BASF Pluracol® 4650 Graft Slabstock Foam Polyol
Description: Pluracol® 4650 polyol is a secondary hydroxyl-terminated graft polyether triol containing approximately 44% solids of copolymerized styrene and acrylonitrile. This polyol has been form..