Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.73 cP @Temperature -10.0 °C |
2.73 cP @Temperature 14.0 °F |
Dynamic, Concentration 0.20 kg FeCl3/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (11 wt% - 20 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |