Physical Properties Metric English Comments
Viscosity 2.60e+6 cP

@Shear Rate 10.0 1/s,
Temperature 230 °C
2.60e+6 cP

@Shear Rate 10.0 1/s,
Temperature 446 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers