Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 2.06e+6 cP @Shear Rate 100 1/s, Temperature 190 °C |
2.06e+6 cP @Shear Rate 100 1/s, Temperature 374 °F |
100 rad/sec; ARES Rheometer |
Dow Engage® ENR 7467.00 Ethylene-Butene Copolymer Description: ENR 7467.00 is a high performance ethylene-butene copolymer, offering superior impact properties for more demanding TPO applications. The polymer has very low crystallinity and is avail.. |