Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 195 cP

@Temperature 60.0 °C
195 cP

@Temperature 140 °F
BASF Pluracol® 1062 Specialty Polyol
Description: Pluracol® 1062 polyol is a high molecular weight, primary hydroxyl terminated diol used in the manufacture of polyurethane shoe soles and fascia products. Pluracol 1062 can also be use..