Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 191300 cP @Shear Rate 500 1/s, Temperature 280 °C |
191300 cP @Shear Rate 500 1/s, Temperature 536 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 93G35DH1 BK549 Nylon 6
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 6 Information provided by DuPont Performance Polymers |