Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 190000 cP @Shear Rate 1340 1/s, Temperature 200 °C |
190000 cP @Shear Rate 1340 1/s, Temperature 392 °F |
ASTM D3835 |
PolyOne Versaflex™ HC MT222 Thermoplastic Elastomer (TPE) Versaflex™ HC MT222 is an exceptionally clear, high performance TPE developed for medical tubing for healthcare. Versaflex™ HC MT222 has been specially formulated without the use of any plasticize.. |