Viscosity 19 cP

@Shear Rate 1000 1/s,
Temperature 290 °C
19 cP

@Shear Rate 1000 1/s,
Temperature 554 °F
Solvay TECHNYL® A 221 PA66, DRY
Description TECHNYL ® A 221 is an unreinforced polyamide 66, medium viscosity, for injection molding, with a special crystallizing agent, for fast cycles. It is available in natural colors. Benef..
Viscosity >= 19 cP

@Time 3600 sec
>= 19 cP

@Time 1.00 hour
V-135-1
Solvay JAGUAR® 413 Surfactant
Description: Nonyl phenol based non ionic surfactant (70 EO)Chemical Name: GALACTOMANNAN BLENDCAS: 39421-75-5; 7631-86-9 Available in: Asia Pacific, Europe, Latin America and North AmericaApplicatio..
Viscosity >= 19 cP

@Time 86400 sec
>= 19 cP

@Time 24.0 hour
V-135-1
Solvay JAGUAR® 413 Surfactant
Description: Nonyl phenol based non ionic surfactant (70 EO)Chemical Name: GALACTOMANNAN BLENDCAS: 39421-75-5; 7631-86-9 Available in: Asia Pacific, Europe, Latin America and North AmericaApplicatio..