Physical Properties Metric English Comments
Viscosity 189000 cP

@Shear Rate 500 1/s,
Temperature 295 °C
189000 cP

@Shear Rate 500 1/s,
Temperature 563 °F
ISO 11403-1 -2
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P..