Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 179600 cP @Shear Rate 500 1/s, Temperature 305 °C |
179600 cP @Shear Rate 500 1/s, Temperature 581 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |