Physical Properties Metric English Comments
Viscosity 170 cP

@Temperature 75.0 °C
170 cP

@Temperature 167 °F
STM 1
Lord Adhesives Thermosetâ„¢ EP-830 Ignition Coil Impregnating and Encapsulation Epoxy
Lord EP-830 is a heat curing, two component epoxy formulation designed especially for use in automotive high voltage ignition coils where adhesion to segmented bobbins is critical. The combination o..
Viscosity 170 cP

@Shear Rate 100 1/s,
Temperature 300 °C
170 cP

@Shear Rate 100 1/s,
Temperature 572 °F
shear rate: 100/s
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..