Polymer Property : Viscosity = 167 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 167 cP

@Temperature 35.0 °C
167 cP

@Temperature 95.0 °F
BASF Pluracol® 1135i Specialty Polyol
Description: Pluracol® 1135i polyol is a nominal 1500 molecular weight triol. Pluracol 1135i has been prepared for applications in flexible slabstock foams and polyurethane adhesive and sealants ap..