Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 161800 cP @Shear Rate 500 1/s, Temperature 270 °C |
161800 cP @Shear Rate 500 1/s, Temperature 518 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3301 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)&l Unreinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3301 NC010 is an unreinforced polytrimethylene terephthalate resin containing 35% renewably sourced ingredients by weight with su.. |