Physical Properties Metric English Comments
Viscosity 150000 cP

@Shear Rate 1000 1/s,
Temperature 290 °C
150000 cP

@Shear Rate 1000 1/s,
Temperature 554 °F
DSM Akulon® F-X9182 PA6
Low/Medium Viscosity
Viscosity 150000 cP

@Shear Rate 5000 1/s,
Temperature 295 °C
150000 cP

@Shear Rate 5000 1/s,
Temperature 563 °F
DAM; ISO 11443
DuPont Performance Polymers Zytel® E42A NC010 Nylon 66  (Unverified Data**)
Zytel® E42A is a high viscosity polyamide 66 for injection molding and extrusion. It has improved break resistance for thick-walled parts.Information provided by DuPont Performance Polymers