Physical Properties Metric English Comments
Viscosity >= 14 cP

@Time 601 sec
>= 14 cP

@Time 0.167 hour
V-135-1
Solvay JAGUAR® 413 Surfactant
Description: Nonyl phenol based non ionic surfactant (70 EO)Chemical Name: GALACTOMANNAN BLENDCAS: 39421-75-5; 7631-86-9 Available in: Asia Pacific, Europe, Latin America and North AmericaApplicatio..
Viscosity 14 cP

@Temperature 40.0 °C
14 cP

@Temperature 104 °F
Teknor Apex TruVis Esters™ DIDA Di-IsoDecyl Adipate