Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 10000 - 13000 cP @Shear Rate 0.100 1/s, Temperature 25.0 °C |
10000 - 13000 cP @Shear Rate 0.100 1/s, Temperature 77.0 °F |
LVF#4, Uncured |
Fibre Glast 180 Clear Gel Coat #180 Clear Gel Coat is a high performance, premium quality gel coat for both airless and air atomized spray applications. #180 offers UV light stability, excellent clarity, crack and chemical resist.. |
|||
Viscosity | 10000 - 13000 cP @Temperature 25.0 °C |
10000 - 13000 cP @Temperature 77.0 °F |
ASTM D445 |
BASF Palamoll® 656 Polymeric Plasticizer Description: Palamoll® 656 is a high viscosity polymeric plasticizer that is compatible with PVC. It is based on adipic acid and polyhydric alcohols. It is resistant to oils, fats, aliphatic hydro.. |