Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 127000 cP @Shear Rate 5000 1/s, Temperature 275 °C |
127000 cP @Shear Rate 5000 1/s, Temperature 527 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Viscosity | 127000 cP @Shear Rate 500 1/s, Temperature 300 °C |
127000 cP @Shear Rate 500 1/s, Temperature 572 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |