Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 123000 cP @Shear Rate 5000 1/s, Temperature 260 °C |
123000 cP @Shear Rate 5000 1/s, Temperature 500 °F |
ISO 11403-1 -2 |