Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 121000 cP @Shear Rate 5000 1/s, Temperature 240 °C |
121000 cP @Shear Rate 5000 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |