Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1202 cP @Temperature 25.0 °C |
1202 cP @Temperature 77.0 °F |
|
BASF Pluracol® 1603 Molded Foam Polyol Description: Pluracol® 1603 polyol is a primary hydroxyl terminated polyether polyol containing an LVI inhibitor package making it ideal for molded seating foam applications. It has an actual funct.. |