Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1200 - 2.00e+7 cP @Temperature 232 - 260 °C |
1200 - 2.00e+7 cP @Temperature 450 - 500 °F |
Average value: 2.16e+6 cP Grade Count:53 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Viscosity | 1200 - 2.00e+7 cP @Shear Rate 50.0 - 100 1/s |
1200 - 2.00e+7 cP @Shear Rate 50.0 - 100 1/s |
Average value: 2.16e+6 cP Grade Count:53 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Viscosity | 1200 cP @Temperature 30.0 °C |
1200 cP @Temperature 86.0 °F |
10% wt, Toluene Solution |
Kuraray SEPTON® S2005 Thermoplastic Rubber SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are hydrogenated styrenic block copolymers, which exhi.. |