Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 114600 cP @Shear Rate 5000 1/s, Temperature 240 °C |
114600 cP @Shear Rate 5000 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |