Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 112800 cP @Shear Rate 5000 1/s, Temperature 250 °C |
112800 cP @Shear Rate 5000 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK695FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |
|||
Viscosity | 112800 cP @Shear Rate 5000 1/s, Temperature 250 °C |
112800 cP @Shear Rate 5000 1/s, Temperature 482 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK695FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK695FR is a 30% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided b.. |