Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 109890 cP @Shear Rate 5000 1/s, Temperature 240 °C |
109890 cP @Shear Rate 5000 1/s, Temperature 464 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® LC6200 BK385 Nylon 612
(Unverified Data**) Toughened Polyamide 612 Developed for ExtrusionInformation provided by DuPont Performance Polymers |