Physical Properties Metric English Comments
Viscosity 104000 cP

@Shear Rate 1340 1/s,
Temperature 200 °C
104000 cP

@Shear Rate 1340 1/s,
Temperature 392 °F
ASTM D3835
PolyOne Versaflex™ VDT 4132 Thermoplastic Elastomer (TPE)
Versaflex™ VDT 4132 is designed to create vibration damping. - Excellent Vibration DampingRear = 350-370F Middle = 375-400F Front = 375-400F Nozzle = 365-380F Screw speed = 100-500rpmPurge thorough..