Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 10.2 cP @Temperature 100 °C |
10.2 cP @Temperature 212 °F |
|
Teknor Apex TruVis Esters™ TNTM TriNonyl Trimellitate |