Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.62e+6 cP @Shear Rate 36.0 1/s, Temperature 275 °C |
1.62e+6 cP @Shear Rate 36.0 1/s, Temperature 527 °F |
ISO 11443 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |