Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.15 cP @Temperature 160 °C |
1.15 cP @Temperature 320 °F |
|
Solvay Chemicals Glycerol alpha monochlorohydrin Viscous liquid used as chemical intermediate.EINECS Number: 202-492-4/CAS Number: 96-24-2/UN number: 2689Information provided by Solvay |