Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.80 cP @Temperature 193 °C |
0.80 cP @Temperature 380 °F |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |
|||
Viscosity | 0.80 cP @Temperature 65.6 °C |
0.80 cP @Temperature 150 °F |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |
|||
Viscosity | 0.80 cP @Temperature 30.0 °C |
0.80 cP @Temperature 86.0 °F |
Dynamic |
Solvay Chemicals Perchloroethylene Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay |