Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Viscosity = 0.66 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 0.66 cP

@Temperature 50.0 °C
0.66 cP

@Temperature 122 °F
Dynamic
Solvay Chemicals Perchloroethylene
Perchloroethylene is a non-flammable productEINECS Number: 204-825-9/CAS Number: 127-18-4/UN number: 1897Information provided by Solvay
Copyright © lookpolymers.com All Rights Reserved