Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 0.070 cP @Temperature 80.0 °C |
0.070 cP @Temperature 176 °F |
Rheology, 2°C/min |
Zyvex Performance Materials Arovex™ 180 Carbon Nanotube Strengthened Prepreg Arovex® 180 Prepreg is a 180°F (82°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Arovex 180 resin contains an optimum level of carbon nanotub.. |
|||
Viscosity | 0.070 cP @Temperature 80.0 °C |
0.070 cP @Temperature 176 °F |
Rheology, 2°C/min |
Zyvex Performance Materials Arovex™ 250 Carbon Nanotube Strengthened Prepreg Arovex® 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (121°.. |
|||
Viscosity | 0.070 cP @Temperature 80.0 °C |
0.070 cP @Temperature 176 °F |
Rheology, 2°C/min |
Zyvex Performance Materials Arovex™ HT 250 Nano-Engineered Composite Prepreg System Arovex® HT 250 Prepreg is a 180°F (82°C) to 280°F (138°C) curing carbon nanotube strengthened epoxy prepreg suitable for numerous composites applications. Normal curing takes place at 250°F (1.. |