Physical Properties | Metric | English | Comments |
---|---|---|---|
Surface Tension | 0.073 dynes/cm @Temperature 0.000 °C |
0.073 dynes/cm @Temperature 32.0 °F |
Concentration 0.15 HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (11 wt% - 20 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |
|||
Surface Tension | 0.073 dynes/cm @Temperature 0.000 °C |
0.073 dynes/cm @Temperature 32.0 °F |
Concentration 0.20 HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (11 wt% - 20 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |
|||
Surface Tension | 0.073 dynes/cm @Temperature 10.0 °C |
0.073 dynes/cm @Temperature 50.0 °F |
Concentration 0.15 HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (11 wt% - 20 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |
|||
Surface Tension | 0.073 dynes/cm @Temperature 10.0 °C |
0.073 dynes/cm @Temperature 50.0 °F |
Concentration 0.10 HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |
|||
Surface Tension | 0.073 dynes/cm @Temperature 20.0 °C |
0.073 dynes/cm @Temperature 68.0 °F |
Concentration 0.05 HCl/kg |
Solvay Chemicals Hydrochloric Acid 31% - Technical Grade (2 wt% - 10 wt% Concentration) Hydrochloric acid, also known as muriatic acid, is a colorless to yellow liquid, with a pungent odor. Hydrochloric acid is a strong acid used as chemical reagent, pH-regulating, ion exchanger regene.. |