Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 97 cSt | 97 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8990 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 97 cSt | 97 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8991MT (UF) Synthetic Oil Information provided by Nye Lubricants. |