Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 9.0 cSt | 9.0 cSt | Base Oil; ASTM D445 |
Nye Lubricants 753G (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.0 cSt | 9.0 cSt | Base Oil; ASTM D445 |
Nye Lubricants 789P (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.0 cSt | 9.0 cSt | Base Oil; ASTM D445 |
Nye Lubricants 798 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.0 cSt | 9.0 cSt | Base Oil; ASTM D445 |
Nye Lubricants 952 (RL) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.0 cSt | 9.0 cSt | Base Oil; ASTM D445 |
Nye Lubricants NPE-UC9 Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.0 cSt | 9.0 cSt | |
ConocoPhillips Hydroclear® 68 Refrigerant Oil Description: Conoco Hydroclear Refrigerant Oil is a high-quality ammonia refrigeration compressor lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Refrigerant Oil is spe.. |
|||
Kinematic Viscosity at 100°C (212°F) | 9.0 cSt | 9.0 cSt | ASTM D445 |
ChevronTexaco ISO 100 Saw Guide Oil FeaturesChevron Saw Guide Oil is manufactured using naphthenic oils and specially selected additives
balanced to reduce friction between saw and guide components in thin kerf saw equipment. These ad.. |