Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 8.57 cSt | 8.57 cSt | ASTM D445 |
ExxonMobil Mobil Vaculine 1409 Mobil Vacuoline 1400 Series oils are extra high performance lubricants specifically designed to satisfy the requirements of machine tools that use one oil for both hydraulic systems and way lubricat.. |
|||