Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 74 cSt | 74 cSt | ASTM D445 |
ChevronTexaco Gear Compounds EP, ISO 1000 Chevron Gear Compounds EP are multipurpose gear lubricants. They provide good thermal stability, extreme pressure protection, antiwear and demulsibility, oxidation, rust, corrosion control and foam .. |
|||
Kinematic Viscosity at 100°C (212°F) | 74 cSt | 74 cSt | |
ChevronTexaco Meropa® 1500 Texaco Meropa oils deliver value through:Gear set efficiencies — High thermal stability EP system maintains clean gear and bearing surfaces, minimizing deposits which interfere with effective lubri.. |
|||
Kinematic Viscosity at 100°C (212°F) | 74 cSt | 74 cSt | Base Oil; ASTM D445 |
Nye Lubricants 762G (NG) Synthetic Oil Information provided by Nye Lubricants. |