Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
Base Oil; ASTM D445
Nye Lubricants 350-SBG-2 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
Base Oil; ASTM D445
Nye Lubricants 377AL (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
Base Oil; ASTM D445
Nye Lubricants 713 (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
ASTM D445
ExxonMobil 46 Mobil EAL Envirosyn H Series
Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper..
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
ASTM D445
ChevronTexaco ParaMount™ 3005 Paraffinic Process Oil
FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur..
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
ASTM D445
ExxonMobil 46 Mobil EAL Envirosyn H Series
Mobil EAL Envirosyn H Series oils are super premium, high performance fully synthetic environmentally aware hydraulic and circulating oils designed to provide outstanding performance in systems oper..
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
ASTM D-445
ConocoPhillips ANDEROL® FGC 20 Synthetic Food Grade Compressor Fluid, ISO 46
Description: ANDEROL FGC Series Compressor Fluids are synthetic hydrocarbon (PAO) based lubricants formulated for use in compressors. FGC Series Fluids meet the former H-1 approval requirements of t..
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
ASTM D445
ChevronTexaco Bright-Cut® AXH Metal Working Fluid
FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components ..
Kinematic Viscosity at 100°C (212°F) 7.8 cSt
7.8 cSt
ASTM D-445
ConocoPhillips ANDEROL® FGH 46 Synthetic Food Grade Hydraulic Fluid, ISO 46