Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Kinematic Viscosity at 100°C (212°F) = 7.4 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ASTM D445
ExxonMobil 447 Mobilmet 440 Series
Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ConocoPhillips Syncon® 46 Synthetic R&O Oil
Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ConocoPhillips SynXPA® 68 R&O Oil
Description: Conoco SynXPA R&O Oil lubricates stationary and portable rotary compressors, as well as reciprocating compressors that operate in severe service. It is useful in single- and double-acti..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ASTM D445
ChevronTexaco Rykon® 5W-20 Premium Oil MV
FeaturesChevron Rykon Premium Oil MV is a versatile multiviscosity lubricant designed to give maximum protection to hydraulic pumps.It is formulated with ISOSYN® base stocks and contains a shear st..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ASTM D445
ChevronTexaco Syntholube® ISO 68 Compressor Oil
FeaturesChevron Syntholube Compressor Oils are synthetic diester-based, oxidation resistant, compressor oils.ApplicationsChevron Syntholube Compressor Oils are used for portable and stationary rotar..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ExxonMobil Mobil ATF D/M
Mobil ATF D/M provides the excellent oxidation and friction stability, anti-wear properties, and low-temperature fluidity desired for most automatic transmissions.Mobil ATF D/M is a super-premium lu..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ChevronTexaco Biostar® Hydraulic 32
Texaco Biostar Hydraulic oils deliver value through:Environmental sensitivity — Readily biodegradable formulation supports use in environmentally sensitive applications.Reduced maintenance — Ashle..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ChevronTexaco Cetus® DE 68
Texaco Cetus DE oils deliver value through:Long life — Texaco Cetus DE oils have a low sludge-forming tendency and a high solvency for deposits that help to keep compressor parts clean. Their abili..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ASTM D445
ChevronTexaco Cetus® PAO 46
Texaco Cetus PAO oils deliver value through:Long lubricant life in high temperature operations — Outstanding thermal and oxidation stability.Extended machinery life and increased compressor efficie..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ASTM D445
ExxonMobil 447 Mobilmet 440 Series
Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m..
Kinematic Viscosity at 100°C (212°F) 7.4 cSt
7.4 cSt
ExxonMobil Mobil ATF D/M
Mobil ATF D/M provides the excellent oxidation and friction stability, anti-wear properties, and low-temperature fluidity desired for most automatic transmissions.Mobil ATF D/M is a super-premium lu..