Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 670 cSt | 670 cSt | Base Oil; ASTM D445 |
Nye Lubricants 774H (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 670 cSt | 670 cSt | Base Oil; ASTM D445 |
Nye Lubricants 774HF (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 670 cSt | 670 cSt | Base Oil; ASTM D445 |
Nye Lubricants 774H-MS (NG) Synthetic Oil Information provided by Nye Lubricants. |