Polymer Property : Kinematic Viscosity at 100°C (212°F) = 63 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 63 cSt
63 cSt
ConocoPhillips Syncon® 680 Synthetic EP Gear Oil, AGMA No. 8EP
Description: Conoco Syncon Synthetic EP Gear Oil is a synthetic polyalphaolefin (PAO) lubricant for enclosed gear sets requiring extreme-pressure gear oils and operating at high temperatures. It is ..
Kinematic Viscosity at 100°C (212°F) 63 cSt
63 cSt
ASTM D445
ChevronTexaco TEGRA® ISO 680 Synthetic Gear Lubricant
FeaturesChevron Tegra Synthetic Gear Lubricants are superior quality industrial EP gear lubricants.The most advanced formulation has been selected to provide superior load carrying and antiwear prop..
Kinematic Viscosity at 100°C (212°F) 63 cSt
63 cSt
See Note 3.
ChevronTexaco Crater® A
Texaco Crater lubricants delivers value through:Low environmental impact — Contains a carrier solvent that is a non-ozone depleting diluent.Good water resistance — Strong resistance to water washo..
Kinematic Viscosity at 100°C (212°F) 63 cSt
63 cSt
ChevronTexaco Pinnacle® EP 680
Texaco Pinnacle EP oils deliver value through:Excellent thermal and oxidation stability — The synthetic hydrocarbon base oils used in these products provide outstanding stability resulting in longe..