Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ChevronTexaco Rando® HD 46 Ashless
Texaco Rando HD Ashless oils deliver value through:Premium performance — Ashless formulation meets or exceeds pump manufacturer requirements for viscosity, rust and corrosion protection, hydrolytic..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ASTM D445
ExxonMobil 798 Mobil DTE 790 Series
Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ConocoPhillips 46 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ConocoPhillips Hydroclear Diamond Class® 46 AW Turbine Oil
Diamond Class AW Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited, antiwear turbine oil developed for use in geared and direct-drive gas turbines and steam turbines in severe ser..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ConocoPhillips Hydroclear Diamond Class® 46 Turbine Oil
Diamond Class Turbine Oil is a premium quality, rust and oxidation (R&O)-inhibited turbine oil developed for use in gas turbines and steam turbines in severe service. It is specially formulated to p..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ConocoPhillips Hydroclear® 46 Refrigerant Oil
Description: Conoco Hydroclear Refrigerant Oil is a high-quality ammonia refrigeration compressor lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Refrigerant Oil is spe..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ASTM D445
ChevronTexaco Clarity® ISO 46 Hydraulic Oil AW
FeaturesChevron Clarity Hydraulic Oils AW are designed to give maximum protection to hydraulic pumps in highperformance industrial applications as well as in environmentally sensitive areas.They are..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ConocoPhillips 46 Ultra-Clean Super Hydraulic Oil
Description: Conoco Ultra-Clean Super Hydraulic Oils have the same high performance characteristics of regular Super Hydraulic Oils with the added advantage of a guaranteed ISO cleanliness code of 1..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ConocoPhillips HD Fleet™ 10W Engine Oil
Description: Conoco HD Fleet Engine Oil is a high-quality, single-grade oil formulated from Conoco's premium hydrocracked base stock and unique additive technology. This oil is highly recommende..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ConocoPhillips Hydroclear® 46 AW Hydraulic Fluid
Description: Conoco Hydroclear AW Hydraulic Fluid is specifically designed for use in high-pressure systems which require greater wear protection and deposit control than that provided by standard a..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ASTM D445
ExxonMobil 46 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ASTM D-445
ConocoPhillips ANDEROL® SAE 20 White Mineral Oil Food Grade Trolley Oil ISO 46
Description: ANDEROL PQ Trolley Oil is a white mineral oil based product that meets the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ Trolley Oil is recomm..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ASTM D445
ExxonMobil 46 Mobil DTE FM Series
Mobil DTE FM Series oils are high performance lubricants designed to satisfy a wide range of multi-use equipment requirements for the food processing and packaging industry. These lubricants are qua..
Kinematic Viscosity at 100°C (212°F) 6.8 cSt
6.8 cSt
ASTM D445
ExxonMobil 798 Mobil DTE 790 Series
Mobil DTE 790 Series lubricants are premium performance turbine oils that are engineered to meet the requirements of the most severe steam turbine designs and operation, with maximum oil charge life..