Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 6.4 cSt | 6.4 cSt | Base Oil; ASTM D445 |
Nye Lubricants 758G (NG) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.4 cSt | 6.4 cSt | ASTM D445 |
ChevronTexaco FM ISO 46 Lubricating Oil Chevron Lubricating Oils FM are premium performance industrial lubricants designed for use in the food processing and other sensitive industries where incidental food contact may occur. Chevron Lubr.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.4 cSt | 6.4 cSt | ASTM D445 |
ChevronTexaco ISO 68 Refrigeration Oil WF FeaturesChevron Refrigeration Oils WF are manufactured using medium viscosity index straight mineral oils. The base stocks are carefully selected to assure the low pour points that are necessary for.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.4 cSt | 6.4 cSt | ASTM D445 |
ChevronTexaco ParaMount™ 2401 Paraffinic Process Oil FeaturesChevron’s ParaMount Paraffinic Process Oils are highly saturated paraffinic process oils with very good color and low aromatic content.Chevron’s modern all-hydroprocessing technology assur.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.4 cSt | 6.4 cSt | |
ChevronTexaco Capella® WF 68 Texaco Capella WF oils delivers value through:Wax-free — Suitable for ultra-low temperature service.Water-free — Low moisture content prevents icing in refrigeration expansion valves and helps pre.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.4 cSt | 6.4 cSt | ASTM D445 |
ExxonMobil 524 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.4 cSt | 6.4 cSt | |
ChevronTexaco Rando® HDZ 32 Texaco Rando HDZ oils deliver value through:High oxidation stability — Longer service life than attainable with conventional lubricants used in high pressure service.Protection against rust and cor.. |
|||
Kinematic Viscosity at 100°C (212°F) | 6.4 cSt | 6.4 cSt | ASTM D445 |
ExxonMobil 524 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |