Polymer Property : Kinematic Viscosity at 100°C (212°F) = 6.0 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 123S (Nyeoil2) Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 362F (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 362HT (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 373 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 375 (RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 390-A(RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 390S-A(RL) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 708D (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants 725A (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants DHL-600 Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants NYEOIL II Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants RP 9901 Rust inhibitor
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8710 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8711 (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
ASTM D445
ExxonMobil 446 Mobilmet 440 Series
Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m..
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
Base Oil
ConocoPhillips Syncon® HP Synthetic Grease NLGI No. 1
Description: Conoco Syncon HP Synthetic Grease is a high-quality, synthetic polyalphaolefin (PAO) lithium grease developed to provide exceptional protection and corrosion resistance for bearings and..
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
ChevronTexaco Transultex® F
Texaco Transultex metalworking fluids deliver value through:Excellent antiweld properties from active sulfur and chlorine which reduce frictional heat, prevent welding of metal to the tool point, ex..
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
ASTM D445
ChevronTexaco Drive Train Fluid HD, SAE 10W
FeaturesChevron Drive Train Fluids HD are high performance lubricants designed for use in transmissions, final drives, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or Allison C4 ..
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
ASTM D445
ExxonMobil 446 Mobilmet 440 Series
Mobilmet 440 Series fluids are high performance, multi-service, non-corrosive straight cutting fluids. They are designed for moderate to heavy duty cutting operations. They are also suitable for m..
Kinematic Viscosity at 100°C (212°F) 6.0 cSt
6.0 cSt
ChevronTexaco SAE 10W Transmission and Drive Train TO-4 Oil
Texaco Transmission and Drive Train TO-4 Oils deliver value through:Longer equipment life — Special additives protect metal surfaces against scuffing and wear even under severe operating conditions..