Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 55.7 cSt | 55.7 cSt | |
ChevronTexaco Thuban® SAE 250 Typical test data are average values only. Minor variations which do not affect product performance are to be expected in normal manufacturing. CPS Number: 220994; MSDS Number: 8801 |