Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8900 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | Base Oil; ASTM D445 |
Nye Lubricants UniFlor 8901 (UF) Synthetic Oil Information provided by Nye Lubricants. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | ASTM D445 |
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | ASTM D445 |
ChevronTexaco Elite-Cut® AM Metal Working Fluid FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | ASTM D445 |
ExxonMobil Exterex™ NP451 Synthetic Fluid Product Description: Esterex™ Polyol Esters are API category Group V fluids. Esterex™ Polyol Esters have excellent lower-temperature properties, good lubricating properties and low volatilities. E.. |
|||
Kinematic Viscosity at 100°C (212°F) | 5.0 cSt | 5.0 cSt | ASTM D445 |
ExxonMobil Mobilarma 522 Mobilarma 500 Series oils are premium performance products primarily intended as run-in or lay-up lubricants, which provide effective rust preventive films on the internal surfaces of machinery. The.. |