Polymer Property : Kinematic Viscosity at 100°C (212°F) = 48.5 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 48.5 cSt
48.5 cSt
ASTM D445
ExxonMobil 634 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..
Kinematic Viscosity at 100°C (212°F) 48.5 cSt
48.5 cSt
ASTM D445
ExxonMobil 634 Mobil SHC 600 Series
Mobil SHC 600 Series lubricants are supreme performance gear and bearing oils designed to provide outstanding service in terms of equipment protection, oil life and problem-free operation. They are ..