Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 41.5 cSt
41.5 cSt
See Note 3.
ChevronTexaco Polystar® Synthetic 4602 NLGI Grade
Texaco Polystar Synthetic 4602 delivers value through:Wide application range — Suitable for high rpm operation, operating temperatures ranging from -40°C to 230°C (-40°F to 446°F) and offers ex..