Physical Properties | Metric | English | Comments |
---|---|---|---|
Kinematic Viscosity at 100°C (212°F) | 41.1 cSt | 41.1 cSt | ASTM D445 |
ChevronTexaco HiPerSYN™ ISO 460 Oil FeaturesChevron HiPerSYN Oils are synthetic compressor, bearing, and gear oils.They provide outstanding thermal and oxidation