Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Kinematic Viscosity at 100°C (212°F) = 40 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants 717AR (RL) Rheolube Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants 755G (NG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants 824A-1 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants PML-S-BLUE Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants PML-W-10 Grease
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8190 (483) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8192 (826-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8192M (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8192R (826RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8921SU (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8923E (717P) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8921 (892-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8921M (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
ASTM D445
ExxonMobil Gargoyle Arctic 234 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
ConocoPhillips 1000 Gear Oil AGMA Lubricant No. 8AEP
Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry..
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants 865 (FG) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8921R (892RP-1) (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
Base Oil; ASTM D445
Nye Lubricants UniFlor 8921S (UF) Synthetic Oil
Information provided by Nye Lubricants.
Kinematic Viscosity at 100°C (212°F) 40 cSt
40 cSt
ASTM D445
ExxonMobil Gargoyle Arctic 234 SHC 200 Series
Gargoyle Arctic SHC 200 Series are fully synthetic, supreme performance lubricants, specifically designed for use in refrigeration compressors and heat pumps. They are formulated from wax-free, synt..
Copyright © lookpolymers.com All Rights Reserved