Polymer Property : Kinematic Viscosity at 100°C (212°F) = 4.9 cSt Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Kinematic Viscosity at 100°C (212°F) 4.9 cSt
4.9 cSt
ASTM D445
ChevronTexaco Elite-Cut® AD Metal Working Fluid
FeaturesChevron -Cut Metalworking Fluids are a complete line of chlorinated cutting oils. The line consists of individual products with antiweld and lubricity properties to cover practically all met..
Kinematic Viscosity at 100°C (212°F) 4.9 cSt
4.9 cSt
ConocoPhillips MV22 Super Hydraulic Oil
Description: Conoco Super Hydraulic Oil is a high-quality antiwear hydraulic fluid formulated from premium Conoco hydrocracked base stocks to provide superior water separation, antiwear protection, ..
Kinematic Viscosity at 100°C (212°F) 4.9 cSt
4.9 cSt
ASTM D445
ChevronTexaco Bright-Cut® NL Metal Working Fluid
FeaturesChevron Bright-Cut Metalworking Fluids are a complete line of chlorine-free cutting oils that offer benefits not found in conventional cutting oils.The unique synthetic antiweld components ..